[00261730]以氟钛酸钾为中间原料的冰晶石 循环制备海绵钛和复合钾的方法

交易价格: 面议

所属行业: 钒钛资源

类型: 专利

技术成熟度: 通过小试

专利所属地:EP欧专局

专利号:2631310

交易方式: 技术转让 技术转让 技术入股

联系人: 四川钒钛产业技术研究院

进入空间

所在地:四川攀枝花市

服务承诺
产权明晰
资料保密
对所交付的所有资料进行保密
如实描述
|
收藏
|

技术详细介绍

项目简介:

The disclosure relates to a method for preparing titanium sponge, and in particular to a method for cyclically preparing titanium sponge and coproducing potassium cryolite using potassium fluotitanate as intermediate material. Titaniferous iron concentrate is the main mineral raw material for extracting titanium. The existing titanium sponge preparation method takes the titaniferous iron concentrate as an initial material, obtains a rich-titanium material through a reducing smelting process, a chlorinated melting process, a pre-reduction hydrochloric acid leaching process or a pre-reduction sulphuric acid leaching process, takes titanium tetrachloride which is formed by reacting the richtitanium material with coke and chlorine gas at a high temperature of about 1000 °C as an intermediate material, and then prepares the titanium sponge through a magnesium thermic reduction process (Kroll process) or a sodium thermic reduction process (Hunter process), wherein the reducing smelting process needs a high temperature of between 1700 and 1800 °C and obtains the rich-titanium material after using coke to perform reduction; the chlorinated melting process needs a high temperature of about 1000 °C and obtains the rich-titanium material after using coke and chlorine gas to perform reaction; the pre-reduction hydrochloric acid leaching process needs to be carried out at a high temperature of about 1200 °C, and uses hydrochloric acid to perform leaching after using coke to perform prereduction, and then heats and dehydrates the titanic acid formed to obtain the rich-titanium material; the pre-reduction sulphuric acid leaching process needs to be carried out at a high temperature of about 1200 °C, and uses sulphuric acid to perform leaching after using coke to perform pre-reduction, and then heats and dehydrates the titanic acid formed to obtain the rich-titanium material. The titanium tetrachloride will generate corresponding coproduct chlorate while preparing titanium sponge through the magnesium thermic reduction process (Kroll process) or the sodium thermic reduction process (Hunter process), and it is necessary to adopt a melting electrolytic method to separate and recycle the metal and chlorine gas.

项目核心创新点:

项目详细用途:

预期效益说明:

项目简介:

The disclosure relates to a method for preparing titanium sponge, and in particular to a method for cyclically preparing titanium sponge and coproducing potassium cryolite using potassium fluotitanate as intermediate material. Titaniferous iron concentrate is the main mineral raw material for extracting titanium. The existing titanium sponge preparation method takes the titaniferous iron concentrate as an initial material, obtains a rich-titanium material through a reducing smelting process, a chlorinated melting process, a pre-reduction hydrochloric acid leaching process or a pre-reduction sulphuric acid leaching process, takes titanium tetrachloride which is formed by reacting the richtitanium material with coke and chlorine gas at a high temperature of about 1000 °C as an intermediate material, and then prepares the titanium sponge through a magnesium thermic reduction process (Kroll process) or a sodium thermic reduction process (Hunter process), wherein the reducing smelting process needs a high temperature of between 1700 and 1800 °C and obtains the rich-titanium material after using coke to perform reduction; the chlorinated melting process needs a high temperature of about 1000 °C and obtains the rich-titanium material after using coke and chlorine gas to perform reaction; the pre-reduction hydrochloric acid leaching process needs to be carried out at a high temperature of about 1200 °C, and uses hydrochloric acid to perform leaching after using coke to perform prereduction, and then heats and dehydrates the titanic acid formed to obtain the rich-titanium material; the pre-reduction sulphuric acid leaching process needs to be carried out at a high temperature of about 1200 °C, and uses sulphuric acid to perform leaching after using coke to perform pre-reduction, and then heats and dehydrates the titanic acid formed to obtain the rich-titanium material. The titanium tetrachloride will generate corresponding coproduct chlorate while preparing titanium sponge through the magnesium thermic reduction process (Kroll process) or the sodium thermic reduction process (Hunter process), and it is necessary to adopt a melting electrolytic method to separate and recycle the metal and chlorine gas.

项目核心创新点:

项目详细用途:

预期效益说明: